FUEL & CHEMICAL PROCESSES ›› 2023, Vol. 54 ›› Issue (2): 8-10.

Previous Articles     Next Articles

Preparation of metallurgical formed coke with high reactivity and high strength by using low-rank coal

  

  1. (2. College of Chemical Engineering, North China University of Science & Technology,Tangshan 063210,China; 3. Xinjiang Ginstar Low Rank Coal Utilization Research Co.,Ltd.,Hami 839000,China)
  • Online:2023-03-23 Published:2023-04-04

Abstract: This paper presents a method for preparing metallurgical formed coke from low rank coal in high proportion. Low rank coal,semi-coke from low rank coal,bituminous coal with some binding capacity and coal asphalt are uniformly mixed and pressed into coal briquette by high-pressure pelletizing machine with linear pressure ≥200 kN/cm. The high-pressure coal briquette becomes metallurgical formed coke after dry distillation at about 1 050 ℃. The test result shows that the compressive strength of the metallurgical formed coke is more than 5 000 N,with CRI 54% and CSR 65%,which can be used as metallurgical coke.

Key words: Formed coke, Low rank coal, Coke reactivity(CRI), Coke strength after reaction(CSR)

CLC Number: