Abstract:
The reason for the low lateral temperature coefficient of coking chamber No.52 of 7.63m coke oven is analyzed.The corbel zone of coking chamber is cleaned under hot state.After cleaning,the lateral temperature coefficient is improved greatly.The coke oven battery gets back to normal production,and the problem of environmental pollution is easier to control.