燃料与化工 ›› 2020, Vol. 51 ›› Issue (2): 34-36.

• 煤焦技术 • 上一篇    下一篇

干熄炉耐火材料修复技术在大修中的应用

蔡明珠1  牟彪2   

  1. 1.中冶焦耐(大连)工程技术有限公司, 大连116085;2.酒钢集团宏兴钢铁股份有限公司焦化厂, 嘉峪关735100
  • 出版日期:2020-03-23 发布日期:2020-03-24

Application of refractory material for major repair on CDQ chamber

Cai Mingzhu1  Mu Biao2   

  1. 1.ACRE Coking & Refractory Engineering Consulting Corporation (Dalian),MCC,Dalian 116085,China; 2.Coking Plant of Jiugang (Group) Hongxing Iron & Steel Co.,Ltd.,Jiayuguan 735100,China
  • Online:2020-03-23 Published:2020-03-24

摘要:

由于干熄焦生产不稳定,造成炉体耐火材料龟裂、剥落、破损严重,需要对干熄炉本体冷却段、“牛腿”、环梁、环形风道内环、炉口及一次除尘器侧墙、高温膨胀节等部位进行维修,以满足正常生产需要。采用传统的砌筑技术砌筑工期长、新旧墙接茬部位膨胀不一致,强度差,采用耐火材料浇筑砌筑技术修复后,新旧墙接茬部位膨胀一致,砌体强度高。

关键词: 干熄炉, 耐火材料, 浇筑砌筑

Abstract:

In the event of unstable CDQ operation,it would cause serious damages to the CDQ chamber refractory,like cracks and flake-offs,which needs a series of repairs,such as on the cooling section of the CDQ proper,bracket,ring beam,inner ring duct,chamber mouth,side wall of the primary deduster and high temperature expansion joint,etc.to meet the requirement for normal production.Since the conventional bricklaying takes longer time,there would be differential expansion between the existing wall and the newly-built,and the joint in between has poor strength.Therefore the new casting technology can repair the joint between the existing wall and the new wall with consistent expansion and with high strength of the brickwork in one piece.

Key words: CDQ chamber, Refractory material, Casting

中图分类号: