摘要:

试验研究了现有型式的炉门砖如何减薄及降低炉门表面散失的热量,试验可知,炉门砖减薄80mm,同时增加新型耐高温隔热板,维修方便,可降低炉门散热造成的热量损失,增加炭化室有效容积,增加焦炭产量,完全能够满足焦炉炉门的需要。

Abstract:

Experiment was carried out to study the methods of thinning the existing oven door brick and reducing heat loss on the surface of oven door.The result shows that if the oven door brick is thinned by 80mm and installed with an additional new type high temperature resistant insulating plate,maintenance of oven door is easier, heat loss on the surface of oven door is less,effective volume of coking chamber is increased and consequently coke output is increased.The thinned brick can meet the requirement of oven door.