REFRACTORIES & LIME ›› 2018, Vol. 43 ›› Issue (1): 17-20.

Previous Articles     Next Articles

Study on the application of magnesia-carbon brick MT-14A in GOR converter bottom

Li Ying1)  Tao Yuting1)  Cao Junqing2)  Zheng Lianying2)  Cao Dali3)   

  1. 1.Haicheng Houying Group, Haicheng 114200, China;
    2.Liaoning Qinghua Refractory Material Co.,Ltd., Dashiqiao 115100, China;
    3.School of Materials Science and Engineering, Shenyang University of Chemical Technology, Shenyang 110142, China
  • Online:2018-02-10 Published:2018-02-10

Abstract:

This paper described the application of magnesia-carbon brick MT-14A in 65T GOR converter bottom and analyzed the sample bricks at the bottom of shorter service life.The results showed that the longest furnace life using 1 000mm-long magnesia-carbon brick MT-14A is 62 times and the average life is 50 times, and that using 800mm-long magnesia-carbon brick MT-14A is 41 times and the average life is less than 30 times.It’s also found that the magnesia-carbon brick MT-14A got fractured in service and proved not a suitable material to be employed in GOR converter bottom since the damage mechanism of MT-14A is melting loss of fused-magnesite and decar-bonization in working surface.

CLC Number: