摘要:

介绍了麦尔兹窑的技术特点,分析了麦尔兹窑连接通道顶部高铝浇注料受损的原因,提出了修复麦尔兹窑连接通道顶部的施工方法,总结了修复施工的注意事项。

关键词: 麦尔兹窑, 连接通道, 浇注料, 修复施工

Abstract:

This paper introduces the technical characteristics of Maerz kiln,analyzes the causes of the damage of the high-alumina castable at the top of the connection channel,puts forward the repair construction method,and summarizes the points for attention in the repair construction.

Key words: