用节能型立窑煅烧30~80mm的小块石灰石,月产生石灰8 000t,石灰CaO含量平均91%,活性度300mL,生过烧率≤8%。获得了可观的经济效益,减少了资源浪费,也降低了生产成本。
Abstract:
The energy-saving shaft kiln calcines the limestone with small grain size ranging from 30mm to 80mm. Its monthly production of lime is 8 000t. The average calcium oxide content in lime is 91%;the reactivity of produced lime is 300mL;both over-burnt and under-burnt rates are ≤8%.Considerable economic benefit is obtained, and the waste of resource and production cost are reduced.
中图分类号:
TQ175.653
王晓阳);秦福礼). 节能型立窑煅烧小块石灰石的实践与体会[J]. 耐火与石灰, 2010, 35(6): 11-12.
Wang Xiaoyang) Qin Fuli).
Practice and perception of energy-saving type shaft kiln for calcination of small grain size limestone[J]. REFRACTORIES & LIME, 2010, 35(6): 11-12.
0 / / 推荐
导出引用管理器 EndNote|Reference Manager|ProCite|BibTeX|RefWorks
链接本文: https://journal03.magtechjournal.com/Jwk3_nhysh/CN/
https://journal03.magtechjournal.com/Jwk3_nhysh/CN/Y2010/V35/I6/11