降低4#和5#麦尔兹窑冶金石灰生过烧率操作实践

李磊   

  1. 柳州钢铁股份有限公司转炉炼钢厂熔剂车间, 柳州545002
  • 出版日期:2015-08-10 发布日期:2015-08-10

Practice on reducing the rate of immature and overcalcined lime of No.4 and No.5 Maerz kilns

Li Lei   

  1. Flux Workshop of Converter Steelmaking Plant of Liuzhou Iron & Steel Co.,Ltd., Liuzhou 545002, China
  • Online:2015-08-10 Published:2015-08-10

摘要:

介绍了在现有低煤气热值状况下,以优化工艺控制,保证设备稳定运行等手段,来降低4#、5#麦尔兹窑冶金石灰生过烧。

Abstract:

This paper introduces the measures of optimizing the process operation and ensuring stable operation of the equipment to reduce the rate of immature and overcalcined lime of No.4 and No.5 Maerz kilns at the condition of low gas value.