耐火与石灰 ›› 2011, Vol. 36 ›› Issue (3): 11-12.

• 综述 • 上一篇    下一篇

麦尔兹窑11m卸料平台温度的控制方法

郭临军 刘志强   

  1. 河北钢铁集团邯钢矿业分公司,邯郸 056201
  • 出版日期:2011-06-16 发布日期:2011-06-16

Brief talk on temperature control method for 11m lime discharge platform for Maerz kiln

Guo Linjun   Liu Zhiqiang   

  1. Hansteel Mining Division of Hebei Iron and Steel Group, Handan 056201, China
  • Online:2011-06-16 Published:2011-06-16

摘要:

根据麦尔兹石灰窑特点,结合邯郸麦尔兹石灰窑生产经验,介绍了当11m卸料平台温度过高时需要检查的设备及采取的相应措施。控制好麦尔兹石灰窑11m卸料平台温度,有利于生产优质产品,并延长石灰窑的使用寿命。

Abstract:

According to the features of Maerz lime kiln and in combination with the production experi ence of Maerz lime kiln of Hansteel, it is described that the equipment needs to be inspected and corre sponding measures are to be taken when the temperature of 11m lime discharge platform is too high. The good temperature control of 11m discharge platform of Maerz lime kiln is favorable to produce high quality product and prolong the service life of the lime kiln.